Lead-Acid Batteries
The Problem
Traditional lead-acid batteries have many defects. This is due to the inherent structural characteristics, which include:
- Plate sulfation
- Active material loss
- Dehydration
- Serious acid polution
- Short cycle life
- Poor low/high temprature characteristics
The Solution
To overcome the structural defects in lead-acid batteries, manufacturers started using AGM and a gel electrolyte bateries. Although this did not solve all the problems, progress was made by:
- Reducing the acid mist
- reducing the water loss rate
- Reducing the self-discharge rate
- Improving the discharge capacity
By solving these problems, a new series of challenges were introduced:
- Poor electrode penetration by the gel electrolyte
- Weak capacity of AGM separator match
- Slow electrode reaction
The Diffrence
In order to overcome the fundamental shortcomings of the lead-acid and AGM or gel batteries, the Lead Crystal Battery uses new proprietary technologies, including:
- Silica crystalline state SiO2 composite electrolyte (not a gel) to replace the conventional sulfuric acid solution
- The preparation method of the Silica crystalline state SiO2 composite electrolyte
- The irrigation fluid device and its battery plus liquid method
- Battery terminals connected to protective devices
- Batteries with liquid shunt valve
- New plates
- New AGM
Diffrence Results
As a result, this self-designed SiO2 cleaning composite electrolyte replaces th conventional sulfuric acid solution/gel. A number of unique and advanced technologies are used in the manufacturing of the Lead Crystal Battery in order to solve the lead-acid/gel battery problems. this includes:
- Virtually no plate sulfation
- No active material loss
- No dehydration
- No acid pollution
- Excellent cycle life
- Very goo low/high temperature characteristics